(1)原材料即带钢卷,焊丝,焊剂。在投入前都要经过严格的理化检验。
(2)带钢头尾对接,采用单丝或双丝埋弧焊接,在卷成钢管后采用自动埋弧焊补焊。
(3)成型前,带钢经过矫平、剪边、刨边,表面清理输送和予弯边处理。(630*10mm,螺旋管壁厚允许偏差表
螺旋钢管规格表|螺旋钢管每米理论重量表
公称外径 nominal O.D
mm
|
公称壁厚 Nominal Wall Thickness mm
|
5.0
|
5.5
|
6.0
|
7.0
|
8.0
|
9.0
|
10.0
|
11.0
|
12.0
|
13.0
|
14.0
|
15.0
|
16.0
|
18.0
|
20.0
|
22.0
|
219
|
26.39
|
28.96
|
31.51
|
36.60
|
41.63
|
|
|
|
|
|
|
|
|
|
|
|
273
|
33.04
|
36.28
|
39.51
|
45.92
|
|
|
|
|
|
|
|
|
|
|
|
|
325
|
39.46
|
43.33
|
47.26
|
54.90
|
62.54
|
70.13
|
|
|
|
|
|
|
|
|
|
|
377
|
45.88
|
50.39
|
54.89
|
63.87
|
72.80
|
81.67
|
|
|
|
|
|
|
|
|
|
|
426
|
51.91
|
57.03
|
62.14
|
72.33
|
82.46
|
92.55
|
102.59
|
|
|
|
|
|
|
|
|
|
457
|
55.73
|
61.24
|
66.73
|
77.69
|
88.58
|
99.43
|
110.23
|
120.98
|
131.60
|
142.34
|
|
|
|
|
|
|
508
|
|
|
74.28
|
86.48
|
98.64
|
110.75
|
122.81
|
134.82
|
146.78
|
158.69
|
|
|
|
|
|
|
529
|
|
|
77.38
|
90.11
|
102.78
|
115.41
|
127.99
|
140.51
|
152.99
|
165.42
|
|
|
|
|
|
|
559
|
|
|
81.82
|
95.29
|
108.70
|
122.07
|
135.38
|
148.65
|
161.87
|
175.04
|
|
|
|
|
|
|
610
|
|
|
89.37
|
104.09
|
118.76
|
133.39
|
147.96
|
162.48
|
176.96
|
191.39
|
|
|
|
|
|
|
630
|
|
|
92.33
|
107.54
|
122.71
|
137.82
|
152.89
|
167.91
|
182.88
|
197.80
|
|
|
|
|
|
|
按照螺旋焊管生产标准的规定,螺旋焊缝钢管的主要检验/控制项目包括:外形尺寸:钢管外径、壁厚、椭圆度、弯曲度、管端垂直度、长度外观质量:焊缝余高、错边、钢管表面、分层、夹杂、焊缝缺陷判定 化学成分 焊接接头拉伸试验 静水压试验 酸蚀检验 无损检验 而直缝焊管没有相应的生产标准。一般螺旋焊管机组均采用在线连续检验方式来保证焊缝的的焊接质量,这是螺旋焊管生产区别于直缝焊管生产的另一重要特征。连续检验有利于焊接缺陷的监控、焊接质量的稳定、焊接等级的保证。由于生产工艺的限制,直缝焊管极难实现连续不间断检验。这将使焊接隐患与质量问题的出现机率增加,甚至影响将来管线运行的整体工作可靠性。 目前江苏省铁废价差在180左右,在性价比上废钢仍有优势。综上所述,不排除下一周继续向上的可能。未来一周依然值得期待,但幅度目前多半有收窄的趋势。临近冬储尾端,钢厂补库需求仍在,加之省内各加工基地、钢厂也都受到疫情影响严重,导致加工基地人员紧张,甚至部分加工基地处于停工状态,这使得废钢供应紧张,造成了近期钢厂到货匮乏的局面。而且短期内加工受阻无法得到缓解,这也短期支撑了废钢价格。而且目前铁废价差180左右,废钢更具优势,综合来看短期江苏废钢市场尚可保持稳中偏强态势,个别钢厂仍有小涨概率,建议近期均匀出货,需随时关注消息面变化。
|